Hello  Tomi

        I suppose some kind of arcing may be there in your system whil
sputtering Aluminium. Possibly some contamination or gap between target
and substrate. So you need to look for that matter also.

At what pressure/volatge you are working?

hope it will help u.

good luck

kamal







     Kamal Kishore                     Phone :(0172) 2237401 to 10
     Engineer,VLSI:FAB                 Ext:576,550,570,441
     Semiconductor Complex Limited.    Fax:(0172)-2236378,2236885
     Sector 72(Indl.Area),S A S Nagar,
     Mohali, Punjab- 160071




On Mon, 5 Apr 2004 [email protected] wrote:

> Send MEMS-talk mailing list submissions to
>       [email protected]
>
> To subscribe or unsubscribe via the World Wide Web, visit
>       http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> or, via email, send a message with subject or body 'help' to
>       [email protected]
>
> You can reach the person managing the list at
>       [email protected]
>
> When replying, please edit your Subject line so it is more specific
> than "Re: Contents of MEMS-talk digest..."
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing