Qing Yao
2004-04-12
Hi,


I have a Nickel structure built on Si substrate using electroless plating. I
was wondering what etchant I could use to etch Si without attacking Ni so
that the Ni structure can be released from the Si substrate.

I'm thinking about using KOH. Does anybody know if KOH will attack Ni? If
so, what is the etch rate? Are there any other choices of etchants (e.g.,
EDP, HNA)?

Thanks!



Best Regards,


Qing Yao
___________________
M&IE @ UIUC



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.