MEMSnet Home: MEMS-Talk: Temporary Bonding for DRIE
Temporary Bonding for DRIE
2004-04-07
Rahul Agarwal
2004-04-08
Burkhard Volland
2004-04-08
BRAD JOHNSON
2004-04-13
Blunier, Stefan
2004-04-13
Krasniansky Vladimir
Temporary Bonding for DRIE
Krasniansky Vladimir
2004-04-13
Hi Brad,
I'm very interesting in temporary adhesives which can handle up to 300
C, but didn't
success to find any. Highest temp that I find - 130 C. Could you tell me
which companies
produces high-temperature temporary glues ?

Sincerely,

Vladimir Krasniansky,

Process Engineer,

Gal-El (MMIC);

100, Yitzhak Hanassi Blvd., P.O. Box 330 Ashdod 77102, ISRAEL.

Tel 972-8-857-2436/4

Fax 972-8-857-2658

[email protected]




 The information contained in this communication is proprietary to Israel
Aircraft Industries Ltd.
and/or third parties, may contain confidential or privileged information, and is
intended only for
the use of the intended addressee thereof. If you are not the intended
addressee, please be aware
that any use, disclosure, distribution and/or copying of this communication is
strictly prohibited.
If you receive this communication in error, please notify the sender immediately
and delete it from
your computer. Thank you.


This message is processed by the PrivaWall Email Security Server.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing