Message: 3
Date: Sat, 10 Apr 2004 20:20:32 -0700
From: "Chunmeng Lu" 
Subject: [mems-talk] fluoroalkyl silane
To: [email protected]
Message-ID: <[email protected]>
Content-Type: text/plain

dear all,
I am trying to use fluoroalkyl silane to get a hydropobic surface on
polyurethane acrylate. could anybody tell me where I can buy it and how can
I use it?
thanks in advance!
Chunmeng Lu


Chunmeng,

Regular methods of fluoro alkylsilane deposition on polymer materials don't
work because of the poor adhesion. Our company has developed special
multi-step vapor deposition method, which allows deposition of hydrophobic
layers on variety of materials, including plastics. Moreover, this method
provides excellent stability of hydrophobic layer in aqueous environments.
Please contact me for further details.

Boris Kobrin, Ph.D.
Director of Technology
Applied MicroStructures, Inc.
4425 Fortran Drive, San Jose CA, 95134
(408) 594-0654
[email protected]



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Harrick Plasma, Inc.
Addison Engineering
MEMS Technology Review