Surface protection during CMP
Jeff Simkins [simkinjr]
2004-04-19
Sri,

Have you tried a vapor coating of wax?

Jeff

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf
Of pskoundinya
Sent: Friday, April 16, 2004 4:24 PM
To: [email protected]
Subject: [mems-talk] Surface protection during CMP

Hi,
When I am polishing one side of a 4-inch Silicon wafer, the other side
of the wafer is ending up with slurry deposits after each polishing
cycle. I am thinking about protecting the other side of the wafer from
slurry deposits and stains by covering it with some adhesive tape that
can be peeled off after entire wafer polishing. This would protect
structures from slurry deposits. Does anyone know of any standard
covering tapes that industry uses to protect the wafer surfaces during
polishing? I would appreciate any suggestions.

Thanks,
SriIndiatimes Email now powered by APIC Advantage. Help!
HelpClick on the image to chat with me
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Harrick Plasma, Inc.