RIE etch rate on dielectric substrate
2004-04-20
Jeff Campbell
RIE etch rate on dielectric substrate
Jeff Campbell
2004-04-20
Hi,

We have noticed that RIE etches on a non-conducting substrate  have a
decreasing (even vanishing) etch rate. A thin unetchable oxide/nitride
layer is the result. Has anyone seen a similar effect? Any suggestions
to overcome this issue?

thanks!

Jeff Campbell