Short circuits thin films capacitors2
2004-04-21
wei chong
Short circuits thin films capacitors2
wei chong
2004-04-21
Hi,

Regarding to the short circuit problem of the thin
films capcitor Si/SiO2/RuO2/Bi3Ti4O12 and
Si/SiO2/Ti/Pt/Bi3Ti4O12, which the Pt, RuO2 and
Bi3Ti4O12 prepared by RF magnetron sputtering.

I prepare the samples in the condition without
cleanroom facilities. Is that this condition will
result in the short circuits problem? The room
humidity is around 60 %.

Thanks!

from,
Chong





__________________________________
Do you Yahoo!?
Yahoo! Photos: High-quality 4x6 digital prints for 25ยข
http://photos.yahoo.com/ph/print_splash


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
The Branford Group
MEMS Technology Review