Thickness Measurements of Silicon Membrane
2004-04-21
Stas Lokshin
2004-04-21
Marc Straub
2004-04-21
Karl Cazzini
Thickness Measurements of Silicon Membrane
Marc Straub
2004-04-21
Stanislav,

Filmetrics sells an inexpensive system that may meet your
needs:

http://www.filmetrics.com/mems.html

There is also some discussion of this issue in the October
and November 1998 MEMS-Talk archives:

http://mail.mems-exchange.org/pipermail/mems-talk/1998-Novem
ber/thread.html


Good luck,

Marc Straub
Solidus Technologies, Inc.
Colorado Springs, CO  USA

-----Original Message-----
From: Stas Lokshin [mailto:[email protected]]
Sent: Wednesday, April 21, 2004 3:26 AM
To: [email protected]
Subject: [mems-talk] Thickness Measurements of Silicon
Membrane


Attn: To all it may concern

Dear Sirs,

Thickness Measurements of Silicon Membrane

We are here in Microsense, Israel are dealing with medical
application. One of the basic parts of our system is Silicon
membrane with following parameters.


On the recent part of our development we need to measure the
membrane thickness.

We would be very obliged if you could advise us any type of
measurements which can be done for this purposes.

Yours faithfully,



Stanislav Lokchine,
Microsense CardioVascular Ltd
Phone: +972-3-644-84-48 ext. 112
Fax:    +972-3-644-45-69



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review
MEMStaff Inc.