MEMSnet Home: MEMS-Talk: silicon nitride passivation for saline solution/water
silicon nitride passivation for saline solution/water
2004-04-22
Alvin Barlian
2004-04-23
๊น€ํ˜„์ˆ˜
2004-04-24
[email protected]
silicon nitride passivation for saline solution/water
Alvin Barlian
2004-04-22
Hi all,
I'd like to operate my device underwater (and most likely saline solution), thus
I need to deposit a passivation layer so that it would protect metal (aluminum)
and the silicon substrate itself. Currently, I have 2500 Angstrom of nitride in
mind (after reading some literatures, I know that nitride is probably the best
passivation scheme in this case). Does anybody know any reference/paper/info on
the thickness of nitride needed in order for the nitride layer to be a good
passivation layer for the metal and the silicon underneath it? Thank you so much
and I greatly appreciate your help and info.

Alvin



---------------------------------
Do you Yahoo!?
Yahoo! Photos: High-quality 4x6 digital prints for 25ยข
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMStaff Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics