I am running some experiments and I have two questions:
1. What other metals (besides Chromium) can I use as adhesion layer for
Platinum?
2. Where can I find some information about HPR 504 fotoresist (I want to
know its viscosity)?

____________________________________________________________________________
_____________
Sebastian Sosin
research assistant
National Institute for Research and Development in Microtechnologies (IMT,
Romania)
ICQ#: 133392471
YM: sosin_sebastian
* Home Tel#:   +4021 771.25.05       E-mail me home

* Mobile Tel#:  +40723.301.581        E-mail me at work

____________________________________________________________________________
_____________



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
MEMS Technology Review
Tanner EDA by Mentor Graphics