MEMSnet Home: MEMS-Talk: Re: Re: STS ASE etch help
Re: Re: STS ASE etch help
2004-04-23
Paul Elliott
2004-04-26
ShuTing
Re: Re: STS ASE etch help
ShuTing
2004-04-26
Hi Paul,

One of the quick and dirty fix would be to have
multiple cycles with different etch:passivation
time ratio combinations. For example, start with
4s:5s -> 5s:5s -> 6s:5s. Problem of this approach
is that you may not have gradual profile transition
between cycles.

Or try to reduce passivation, i.e. reduce C4F8 flow.
You can try to change the power, but I would start
with the flow. This may cause bowing. (instead of nice
and straight negative profile) But you should be able
to have larger backside CD. This is the general
direction I would go for. I would recommend you to run
a mini DOE to find the process window before start
fine tuning the recipe.

Good luck!

ShuTing



ShuTing Hsu
Graduate Student Researcher
Integrated Photonics Laboratory
UCLA EE Department
420 Westwood Plaza, 63-128 Eng 4
Los Angeles, CA 90095
Tel:   (310) 825-7338
Fax:  (310) 794-5513
Email:  [email protected]



-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
Paul Elliott
Sent: Friday, April 23, 2004 11:54 AM
To: [email protected]
Subject: [mems-talk] Re: Re: STS ASE etch help



Can you advise any parameters to control sidewall angle of a 500um thru
wafer etch?  I need to obtain a negative sidewall profile no greater
than 1
degree across a 4" substrate with varying diameters(~150um dia.).

Eric Miller  advised maybe the ICP power and/or
the
pressure are major contributors.

My intial posting is below.

Thanks in advance for any advice,
Paul

Sent: Tuesday, February 10, 2004 7:02 AM
Subject: [mems-talk] DRIE sidewall angle


>What is the expected tolerance for sidewall angle when DRIE 'etching a
>Si substrate 500um thick?
>
>I need to etch an arrayed die pattern consisting of two holes 125um and
>155um diameter.  The two holes are spaced 150 um apart and the die are
~1mm
>apart.  I want to etch 125 um diameter hole through the 500um thick
>wafer and obtain a negative sidewall profile no greater than 1 degree
>and a backside hole diameter of 125um +17um / -0um.  Likewise, I need
>the 155um diameter hole to have a negative sidewall profile no greater
>than 1 degree and a backside hole diameter of 155um +17um / -0um.
>
>Thank you in advance for any guidance,
>
>Paul

_________________________________________________________________
Test your 'Travel Quotient' and get the chance to win your dream trip!
http://travel.msn.com


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics