A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RE: cantilever beams experimental data
RE: cantilever beams experimental data
2004-04-30
Maximiliano Fischer
RE: cantilever beams experimental data
Maximiliano Fischer
2004-04-30
Hello,

I'm Maximiliano Fischer. I work in MEMS in Argentina. My thesis work in
Purdue University, Indiana, USA was to create a mechanical test for a
metallic membrane, the only moving part of a Raytheon's RF MEMS Switch.
Regarding mechanical issues, I can reccomend looking for these authors:

William Sharpe Jr., PhD (for tensile tests in metals and polysilicon),
Stephen Senturia, PhD (for his famous M-Test, which will be of great
interest to you since it actuates a fixed-fixed beam electrostatically),
Horacio D. Espinosa, PhD (with whom I worked on mechanical characterization)

I hope to be of any help. Regards!

Maximiliano



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.
Addison Engineering