Hello,

I'm making process where I would like to evaporate Ti/Pt/Au on GaAs/AlGaAs
system and use Ti/Pt/Au as a RIE etch mask. However ion-bombardment in RIE
damages my Au layer and causes sputtering of Au around my sample.

I was thinking that it could be possible to have Cr as a mask layer so I
would evaporate Ti/Pt/Au/Cr and use that as a etch mask. However after RIE
etch I should be able to strip Cr without damaging GaAs / AlGaAs layers or
my Ti/Pt/Au. Actually I can live with some damage to metals or AlGaAs but
GaAs can't be etched in any way.

Do you any good formulations for Cr stripping that would be selective on
GaAs / AlGaAs and Ti/Pt/Au?


Best regards,
-Jukka Viheriala




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
The Branford Group
Mentor Graphics Corporation