Rajeshuni Ramesham
1998-10-26
Rajeshuni Ramesham
Re: electroplating bath
Rajeshuni Ramesham
1998-11-10
Transene Inc., In Boston, MA. Ramesham

At 10:02 AM 10/27/98 +0100, you wrote:
>You may ask
>
>Doduco GmbH & Co.
>Im Altgefaell 12
>D-75181 Pforzheim, Germany
>Fax ++49-7231-602398
>
>Doduco is one of Europe's most established manufacturers of galvanic
>baths and can certainly provide you with what you need.
>
>>
>> Does any one know electroplating suppliers that sells small or
>> modest quantities of electroplating bath for research purposes?
>>
>> Cha-Mei Tang
>Yours sincerely, Kai Hiltmann
>
>mailto:[email protected]    http://www.IMIT.Uni-Stuttgart.de
>K. Hiltmann
>c.o. HSG-IMIT
>Sensorics Section
>W.-Schickard-Str. 10
>D-78052 Villingen-Schwenningen
>
>Phone ++49-7721-943-236
>Fax   ++49-7721-943-210
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics