MEMSnet Home: MEMS-Talk: Processing of 260micron SU8 layer.
help:minimum gap for waveguide devices?
2004-05-06
Yinlan Ruan
Processing of 260micron SU8 layer.
2004-05-07
[email protected]
2004-05-07
NIU Xize
Processing of 260micron SU8 layer.
NIU Xize
2004-05-07
Dear Christian Antonio,

I got 240 um layer by double coating of SU8-2025, not very easy to
control, but better than using 2150. The exposure time depends on your UV
intensity. I used 50 seconds with UV intensity 20mJ/cm^2.

Best


X.Z. Niu

Department of Mechanical Engineering
The Hong Kong University of Science & Technology
Clear Water Bay, Kowloon, Hong Kong


> Hello All,
>
> I was wondering whether anyone can help me.  I am currently processing
> 260micron  SU8-2100 layers on Silicon substrates.  I have tried the
> suggested procedure by  microchem but did not get the results I wanted.
> I have also gotten procedures from  other groups in the literature but
> many are quite different to each other.  I am especially  concerned
> about the exposure times which varies a lot from different groups.  Has
> anyone had experience in processing layers this thick with good results
> and could share  their procedure or experiences.
>
> Any input will be greatly appreciated.
>
> Thank you.
>
> Christian Antonio
> Research Student
> Industrial Research Institute Swinburne,
> Australia.
>
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Harrick Plasma, Inc.
Addison Engineering