A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: photo-patternable PDMS
photo-patternable PDMS
2004-05-12
Tushar Bansal
2004-05-13
Z.,W.Y.(Lydia)
Generating fine dots for Photogrammetry
2004-05-13
ramji dhakal
2004-05-14
Robert Black
photo-patternable PDMS
Z.,W.Y.(Lydia)
2004-05-13
Hi, Tushar,

I tried to repeat this experiment for a long time. I did not get a good pattern
neither.

Both pre-exposure bake and post-exposure bake are required since the mixture is
negative-photoresistance type material.

I usually disolve the DMAP into Xylenes and then pour the DMAP+Xylenes mixture
in to PDMS.

I got help form this discussion group to change DMAP to other photoiniatior to
match the UV wavelength of my aligner. Otherwise, exposure time will be 1 hour
or more.

I have use Sylgard 184 (Dow Corning) and RM-033(Gelest).Actually, the amounts
of each chemical to use have been reported in several papers and this discussion
group. PDMS : Xylenes : DMAP = 100:2:1 (weight ratio)

Just recently, Dow Cornning has a new product, photopatternable spin-on
silicone. Please check its website to see whether it is suitable for your
application.

Good luck

Lydia



Quoting Tushar  Bansal :

> Hello Everyone,
> I am trying to make photopatternable PDMS. I am using methacrylate
> terminated PDMS and mixing it with Xylenes and DMAP (DMAP is the
> photoinitiator, Xylenes is a thinner). This solution was reported in
> several papers. However, it is polymerizing far too quickly and the DMAP
> is not dissolving. Furthermore, on exposure and development, no actual
> pattern is observed. Are we missing a step in this procedure? The amounts
> of each chemical to use were not reported in the papers.
>
> Please suggest any missing steps to the above procedure or any alternate
> procedures to achieve a photo patternable PDMS.
>
> Thanks,
> Tushar
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>




-------------------------------------------------
This mail sent through IMP: http://horde.org/imp/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
Tanner EDA by Mentor Graphics
MEMS Technology Review