MEMSnet Home: MEMS-Talk: refraction index of LPCVD silicon dioxide
refraction index of LPCVD silicon dioxide
2004-05-14
Qing Yao
2004-05-14
X. Yuan
2004-05-14
Shile
2004-05-17
Feridun Ay
2004-05-14
Michael D Martin
2004-05-15
Gert Eriksen
2004-05-17
Glenn Silveira
50 +/- 5 micron through hole in Pyrex wafer
2004-05-17
Patrick Roman
2004-05-18
Zheng Xia
2004-05-18
David Nemeth
refraction index of LPCVD silicon dioxide
Qing Yao
2004-05-14
Hi,


I was wondering if some one could tell me the typical value of refraction
index of LPCVD Silicon Dioxide. It is deposited at about 420 degrees
centigrade on a silicon wafer. I use a focus ellipsometer to measure its
thickness. I tried 1.46 but got very large fit error (about 500). Please let
me know if you have any information about this. Thanks!


Best Regards,


Qing Yao
___________________
M&IE @ UIUC



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
University Wafer