Residue remover of RIE polyimide on Al metallization
2004-05-25
Nels P. Ostrom
2004-06-20
David Ovrokzky
Electrophoretic deposition
2004-06-21
David Ovrokzky
Residue remover of RIE polyimide on Al metallization
Nels P. Ostrom
2004-05-25
I have encountered this problem also.  It looks like a black
or grey "soot" on the bottom.  It is not stuck to the bottom
of the features, and is moved when an alpha-step tip is
dragged across it.  In the past, I have cleaned the "soot"
from my features in an ultrasonic tank with either water or
solvents like acetone.  It actually works pretty well.  On
some occasions, I have had to iterate between the RIE and the
ultrasonic agitation because the "soot" acts as a mask.  I
have attempted to change settings on the RIE in order to
reduce the effect but I did not have any luck.  Hope this
helps.

---- Original message ----
>Date: Mon, 24 May 2004 17:14:18 -0700
>From: "Honggang Jiang" 
>Subject: [mems-talk] Residue remover of RIE polyimide on Al
metallization
>To: "General MEMS discussion" 
>
>Hi all:
>I encountered a problem while doing RIE polyimide (85%O2+15%
CF4) to expose
>the underlying Al metallization. It was found that some
residues were
>generated on top of the exposed Al after RIE etching. Does
anybody know what
>chemicals can be used to remove these residues without
attacking the exposed
>Al metal. Thank you very much.
>
>========================================
>Honggang Jiang
>Materials Science Engineer
>Second Sight
>12744 San Fernando Road
>Building 3
>Sylmar, CA  91342
>Ph: 818 833 5058
>Fx: 818 833 5067
>========================================
>
>IMPORTANT NOTICE:
>This email is confidential, may be legally privileged, and
is for the
>intended recipient only.  Access, disclosure, copying,
distribution, or
>reliance on any of it by anyone else is prohibited and may
be a criminal
>offense.  Please delete if obtained in error and email
confirmation to the
>sender.
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change
your list
>options, visit http://mail.mems-
exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing
services.
>Visit us at http://www.memsnet.org/

Nels Ostrom
[email protected]
Graduate Research Assistant
Optical Physics and Engineering
Dept. of Electrical and Computer Engineering


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing