MEMSnet Home: MEMS-Talk: TEOS in Hot Phos?
TEOS in Hot Phos?
1998-11-25
James Freese
TEOS in Hot Phos?
James Freese
1998-11-25
Does anyone know how much TEOS gets etched in a Hot Phosphoric bath ~160 C. I
am specifically worried about LPCVD TEOS and it's etchrate in this bath, but
any TEOS info would be helpful.
Jim Freese