mahdi bagheri
2004-06-04
Hi everybody,

I want to create a silicon micromembrane. I`m using a
~1 micron thermal SiO2 as a masking layer for KOH
etching.
There is a problem that I can`t overcome, when I want
to etch SiO2 to create windows, HF removes photoresist
layer before creating the layout.
I will be thankful if anybody can help me.

Mahdi Bagheri




__________________________________
Do you Yahoo!?
Friends.  Fun.  Try the all-new Yahoo! Messenger.
http://messenger.yahoo.com/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing