Hi everybody,
             Does anybody know a good supplier for Cr etchant or knows the
recipe for it? I'm looking for a Cr etchant that can etch Chromium without
attacking Nickel at the same time.


With kind regards,

Didier.

---
PhD student.

Singapore Synchrotron Light Source (SSLS)
5 Research Link,
Singapore 117603

Email: slsbdfc at nus dot edu dot sg
Web: http://ssls.nus.edu.sg





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Harrick Plasma, Inc.