MEMSnet Home: MEMS-Talk: Question: Electroless Nickel on dielectric
Question: Electroless Nickel on dielectric
2004-06-10
Hiren Thacker
2004-06-23
#GUO XUN#
Question: Electroless Nickel on dielectric
#GUO XUN#
2004-06-23
Hi,



In my lab, my friend used a method different from yours to plating a Ni
layer on polymer film. But not trying on SiO2 or Silicon Nitride. But I
am figuring that his method should be working.



Check the paper "Electroless Nickel-Plated UV-Embossed Microstructured
Surface with Very High Aspect Ratio Channels" in Langmuir



Good luck



Samuel


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
MEMStaff Inc.
Process Variations in Microsystems Manufacturing