MEMSnet Home: MEMS-Talk: corner compensation structure for 100 Si in KOH
corner compensation structure for 100 Si in KOH
2004-06-21
Nibras Sahib Awaja
2004-06-23
Michael L
corner compensation structure for 100 Si in KOH
Michael L
2004-06-23
Hi,

Have a look at the following reference:

"Corner compensation techniques in anisotropic etching of 100-silicon using
aqueous KOH", Sandmaier, H.; Offereins, H.L.; Kuhl, K. & Lang, W., IEEE,
1991, pp. 456-459.

These authors have a few papers on corner compensation so do a literature
search and you should be able to track down some more useful papers. You can
download the above article on IEEE Xplore.

Regards,

Michael Larsson


>From: "Nibras Sahib Awaja" 
>Reply-To: General MEMS discussion 
>To: [email protected]
>CC: [email protected]
>Subject: [mems-talk] corner compensation structure for 100 Si in KOH
>Date: Mon, 21 Jun 2004 10:53:25 +1000
>
>Dear all,
>I am trying to add a compensation structure to the convex corner of <100>Si
>spring and etch it in KOH+water. Could you please advice me about how can I
>choose the right dimension of these structure.
>Cheers,
>Nibras
>
>-----Original Message-----
>From: [email protected]
>To: [email protected]
>Date: Mon, 21 Jun 2004 02:00:51 +1000 (EST)
>Subject: MEMS-talk Digest, Vol 20, Issue 22
>
>Send MEMS-talk mailing list submissions to
>       [email protected]
>
>To subscribe or unsubscribe via the World Wide Web, visit
>       http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>or, via email, send a message with subject or body 'help' to
>       [email protected]
>
>You can reach the person managing the list at
>       [email protected]
>
>When replying, please edit your Subject line so it is more specific
>than "Re: Contents of MEMS-talk digest..."
>
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

_________________________________________________________________
Express yourself with cool new emoticons http://www.msn.co.uk/specials/myemo


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Addison Engineering
Mentor Graphics Corporation