MEMSnet Home: MEMS-Talk: SU 8 Photoresist
SU 8 Photoresist
2004-06-24
Yeswanth Rao
2004-06-25
Patrick Poissant
2004-06-30
Lee, Duhyun
2004-06-25
Brubaker Chad
SU 8 Photoresist
Brubaker Chad
2004-06-25
Yeswanth,

Su-9 2025 is 69% (wt/wt) solids, while the SU-8 2002 is ~40% solids. Therefore,
to match the SU-8 2002, you'd need to dilute 100g of SU-8 2050 with 72g of SU-8
thinner (make sure it is cyclopentanone, and not GBL, which will cause a shift
in your results).  For a 1.7 µm coat, you'd probably be safe with 75-80 g of
thinner.

Best Regards,

Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel: (602) 437-9492, Fax: (602)437-9435 e-mail:
[email protected], www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.

 -----Original Message-----
From:   [email protected] [mailto:[email protected]]  On
Behalf Of Yeswanth Rao
Sent:   Thursday, June 24, 2004 9:01 AM
To:     [email protected]
Subject:        [mems-talk] SU 8 Photoresist

Dear All,



I would like to use SU 8 photoresist to get a uniform coating of 1.7
micron on Si and Si/Cr. I have SU-8 2025 photoresist and SU 8 thinner.
Would it be possible to use this thinner to reduce the viscosity of the
2025 resist to get down to 1.7 micron thickness? If that is possible,
would anyone be able to able to guide me as to what should be ratio of
this mixture to achieve this thickness. Thanks in advance



Yeswanth L Rao

Graduate Research Assistant

Micro/Nano Fabrication Laboratory

Driftmier Engineering Center

University of Georgia

Athens, GA 30602

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
University Wafer
Mentor Graphics Corporation