MEMSnet Home: MEMS-Talk: Plasma etching of thin PDMS layer
Plasma etching of thin PDMS layer
2004-07-04
[email protected]
2004-07-04
Z.,W.Y.(Lydia)
SU-8 Removal
2004-07-04
Tingrui Pan
2004-07-05
Edward Blackwell
2004-07-06
Greg Reimann
Plasma etching of thin PDMS layer
Z.,W.Y.(Lydia)
2004-07-04
Hi, Zou,

Geogergtown University group said 75% CF4 and 25% O2 gave the highest etch rate.


J. Garra, T. Long, J. Currie, T. Schneider & R. White, M. Paranjape; J. Vac.
Sci. Technol. A vol. 20, no. 3, May/ June, pp 975-982. (2002)

Good luck!

Lydia


Quoting [email protected]:

> Hi,
>
> We want to blanket-etch a thin PDMS layer (1~2um thick) with
> CF4/O2 plasma.  Can anyone suggest a suitable gas mixture,
> power, pressure and also the associated etch rate?
>
> Thanks a lot!
>
> Jun
>
> *******************************************
> Jun Zou
> 319B Micro and Nanotechnology Lab
> University of Illinois at Urbana-Chamapaign
> 208 N. Wright St.
> Urbana, IL 61801
> Phone: (217)265-0808
> Fax: (217)244-6375
> *******************************************
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>




-------------------------------------------------
This mail sent through IMP: http://horde.org/imp/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMStaff Inc.
Addison Engineering