MEMSnet Home: MEMS-Talk: mechanical properties of Si vs. oxygen concentration
mechanical properties of Si vs. oxygen concentration
2004-07-07
Albert K. Henning
mechanical properties of Si vs. oxygen concentration
Albert K. Henning
2004-07-07
Hello,

I have seen some oblique references in the literature to the dependence
of silicon mechanical properties upon oxygen concentration.  I would
appreciate any detailed references which the readers of MEMS-Talk might
offer.

Best regards,

Al Henning

--
Albert K. Henning, Ph.D.
Director of Technology                650-617-0854
Redwood Microsystems, Inc.            650-326-1899 (FAX)
959 Hamilton Avenue                   [email protected]
Menlo Park, CA  94025                 http://www.redwoodmicro.com







reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMS Technology Review