MEMSnet Home: MEMS-Talk: Su-8 craking problem
Su-8 craking problem
2004-07-13
Amani Salim
2004-07-14
#GUO XUN#
2004-07-14
Brubaker Chad
2004-07-14
Michael L
Tin etchant
2004-07-14
Robert Dean
Su-8 craking problem
Amani Salim
2004-07-13
Dear colleagues,

Any suggestions for avoiding cracking in Su8?
am using the 2100 Su8, and am making 100 microns features and follow
exactly the recipe suggested by microchem, seems like theres still small
cracks at the border of my 10 microns structures,

any suggestions are very helpful,

regards,



Amani Salim
******************************************
Research Assistant
Department of Electrical and Computer Eng.
U of Minnesota,T.C.
UMBM Lab
Office phone: 612 626-0590
Lab phone: 612-626-7188


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
MEMStaff Inc.