Hi, all,

Does anyone have experience with spining conductive
epoxy on silicon wafer? Epotek E4110-LV has low
viscosity property(500cPs, 100rpm/23C)which is
comparable to epoxy 330. But I am not sure this paste
can be spun on uniformly. Any suggestion will be
greatly appreciated.

Thanks,
Jianzhong




__________________________________
Do you Yahoo!?
New and Improved Yahoo! Mail - 100MB free storage!
http://promotions.yahoo.com/new_mail

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Addison Engineering