Security consideration when working with chlorated gas
2004-07-13
Francois Montaigne
Security consideration when working with chlorated gas
2004-07-14
Cyrille Hibert
Security consideration when working with chlorated gas
Cyrille Hibert
2004-07-14
GRC Edwards system is a solution.
Check that pdf p.10 http://www.bocedwards.com/pdf/clearchoice.pdf
Feel free to contact me directly if you need more info.
Regards,
Cyrille.

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Francois Montaigne
Sent: 13 July 2004 16:45
To: [email protected]
Subject: [mems-talk] Security consideration when working with chlorated
gas


Hello
We are currently using a RIE machine with mainly SF6 and CHF3. We are
considering to used gas containing chlore or even brome. Which specific
equipment is required concerning the evacuation and the safety when working
with such gas? Is there some resource available online about this subject?
Thanks for yours answers
Regards
Francois

___________________________________________________________
Dr François Montaigne
Laboratoire de Physique des Matériaux - UMR 7556
Faculté des Sciences - Université Henri Poincaré - Nancy I
Bd des aiguillettes B.P. 239
54506 VANDOEUVRE LES NANCY Cedex
FRANCE
Tel: +33 3.83.68.48.08
Fax: +33 3.83.68.48.01

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Nano-Master, Inc.