SAW delay line testing
2004-07-13
Yeswanth Rao
2004-07-14
Wieslaw Bicz
SAW delay line testing
Wieslaw Bicz
2004-07-14

Yeswanth Rao wrote:

>I have fabricated a SAW (surface acoustic wave) device and would like to
>use it as a delay line sensor. I have a Network Analyzer (HP E8801A).
>Can anyone provide some information on how to connect my device with the
>network analyzer for testing? Any information on how to make a test set
>up will be helpful. Thank you.
>
>
>
>Yeswanth L Rao
>
>Graduate Research Assistant
>
>Micro/Nano Fabrication Laboratory
>
>
>
It is much simpler to use pulse or burst generator and a scope.
One transducer should be connected to the pulser and the second to the scope.
You must be able to see signal after the delay, that you expect.

What is the frequency of your delay line?



Wieslaw Bicz

---------------==========   OPTEL sp. z o.o.   ===========---------------
------===== R&D: Ultrasonic Technology/Fingerprint Recognition ====------
ul. Otwarta 10a PL 50-212 Wroclaw Tel.:+48 71 3296854 Fax.:+48 71 3296852
--------==== mailto:[email protected]  -=-  http://www.optel.pl ====-------



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review