MEMSnet Home: MEMS-Talk: wafer post polish cleaning
wafer post polish cleaning
2004-07-20
Yilei Zhang
2004-07-20
Gary
wafer post polish cleaning
Yilei Zhang
2004-07-20
Hi colleagues:
Can anybody provide info. about the post cleaning process to remvoe particles
after wafer polishing? I ued colloidal silica polishing subspension to polish
my wafer with 2um silica layer. I just want to remove a very thin layer of
silica, not all the silica layer. After polishing, there are lots of particle
left, which cannot be removed by ultrasonic cleaning with Acetone. Any
suggestion will be appreciated.

Regards,
Yilei Zhang








reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Tanner EDA by Mentor Graphics