Platinum etch
Imran Ghauri
2004-07-26
Hi,

Can anyone help me in finding

1) the best recipe for the wet etch for Platinum which
can stand standard  photoresist (AZ 4330).

2)Also, I want to create some rectangular shape
(1mmx1mm) cavities of about 20 microns deep. Can
anyone help me in this regard too. I've on my one
wafer devices with metal combinations Pt/Ti and on
other wafer devices Pt/Cr and third wafer with Ti/Cr.
Will it be feasible to create cavities before or after
fab process. Any suggestions will be appreciated.

imran
[email protected]
Grad Student




__________________________________
Do you Yahoo!?
New and Improved Yahoo! Mail - 100MB free storage!
http://promotions.yahoo.com/new_mail

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
The Branford Group