MEMSnet Home: MEMS-Talk: need help on making pyramid array on the ceramic thick film
need help on making pyramid array on the ceramic thick film
2004-07-26
WENYI ZHU
need help on making pyramid array on the ceramic thick film
WENYI ZHU
2004-07-26
Dear all,
I am trying to make some pyramid array on the ceramic thick film about 25
micrometers to 100 micrometer thick.I found a method  called anisotropic
etching in KOH can make pyramid cavity on the  <100> single crystal si
wafer,but my etching object is isotropical ceramics,for example BST(Barium
strontium titanate).It is a kind of polycrystal material.Is there any other
method to make these pyramids in such fine scale?
You will be highly appreciated you if you can give me any suggestions.
Thanks a lot!

peggy


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMStaff Inc.
The Branford Group