2004-08-04
You can use Thermo Couple (TC) wafers to calibrate your wafer temp. You can
contact SensArray Corporation for TC wafers.

"Tan, Chuan Seng"  wrote:
Hi All,

Does anyone know how to determine the wafers temperature during metal
deposition in an e-beam chamber ?

Thanks for your inputs.

Chuan Seng

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


(Pramod Gupta)
21084 Red Fir Court
Cupertino, CA 95014
Phone: (408) 253-1646


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
Tanner EDA by Mentor Graphics
The Branford Group