Hi Tan

        Normally a thermocouple is located near to the substrate holder in
the evaporation system.This shows not the actual temp of substarte but is
close enough.








     Kamal Kishore                     Phone :(0172) 2237401 to 10
     Engineer,VLSI:FAB                 Ext:576,550,570,441
     Semiconductor Complex Limited.    Fax:(0172)-2236378,2236885
     Sector 72(Indl.Area),S A S Nagar,
     Mohali, Punjab- 160071




On Wed, 4 Aug 2004 [email protected] wrote:

> Send MEMS-talk mailing list submissions to
>       [email protected]
>
> To subscribe or unsubscribe via the World Wide Web, visit
>       http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> or, via email, send a message with subject or body 'help' to
>       [email protected]
>
> You can reach the person managing the list at
>       [email protected]
>
> When replying, please edit your Subject line so it is more specific
> than "Re: Contents of MEMS-talk digest..."
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.