Pyrex CTE at 500C
2004-08-24
Paul Elliott
2004-08-26
Carsten Wesselkamp
Pyrex CTE at 500C
Carsten Wesselkamp
2004-08-26
Dear Paul,

I have a chart which specifies relative expansion over temperature for 0 to
600 degrees Celsius. Please contact me directly and I can send it by e-mail.

Best regards,

Carsten Wesselkamp
Plan Optik GmbH
Unter den Eichen
56479 Elsoff / Germany

P.S.: Plan Optik produces glass wafers (from Pyrex or other materials) for
MEMS and semiconductor applications.

------------------------------

Message: 2
Date: Tue, 24 Aug 2004 13:27:32 -0400
From: "Paul Elliott" 
Subject: [mems-talk] Pyrex CTE at 500C
To: [email protected]
Message-ID: 
Content-Type: text/plain; format=flowed

Does anyone have the Coefficient of Linear Thermal Expansion for Corning
Pyrex 7740 at 500 degrees C?

Current data is 3.25 through 300 degrees C.

Thanks for your help,

Paul

_________________________________________________________________
Don’t just search. Find. Check out the new MSN Search!
http://search.msn.click-url.com/go/onm00200636ave/direct/01/




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
MEMStaff Inc.
Addison Engineering