2004-08-31
Chen-Han Lee
2004-08-31
Anthony Cooper
2004-08-31
Michael Cooke
2004-08-31
Flavio Giacomozzi
2004-09-01
vijay j
2004-08-31
Kasman , Elina
2004-08-31
[email protected]
adhesion between Si wafer and gold film
vijay j
2004-09-01
hai,


   Since the surface free energy of gold will not match with silicon thats why
adhesion is poor. use the chromium as barrier between gold and silicon.....


bye,
regards,
vijay.

Chen-Han Lee  wrote:



Dear all,

could anyone help me please.
I am doing some electroplating using SU-8 mould.
gold is evaporated before SU-8 is deposited.
after the developing step,
many SU-8 parts fall off of the wafer with gold film attached to them,
how do i improve the adhesion between Si and the gold film,
so that i have a a complete patterned wafer??

thanks for the help.

Chen han

///////////////////////////////////
Chen-Han Lee
Research Student
School of Manufacturing and Mechanical Engineering,
University of Birmingham,
Birmingham, B15 2TT
United Kingdom,
Phone : +44 121 4144245
Fax : +44 121 4143958
E-Mail : [email protected]
///////////////////////////////////


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

Yahoo! India Matrimony: Find your life partneronline.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
University Wafer
Nano-Master, Inc.