For Eagle NT90 users,

I have been trying to remove this Eagle NT90 resist after sequential dry and
wet etching. I have found it is impossible to remove by long 35W plasma
etching and other resist stripper (N-METHYL-2-PYRROLIDONE). I do not have the
Eagle resist remover and would only consider it if there is no other way to do
it. I would prefer not to use other conventional remover if possible. Does
anyone know a way to solve this?

Thanks in advance!

MY


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
MEMStaff Inc.
Process Variations in Microsystems Manufacturing