Joolien Chee
2004-09-02
Robert Black
2004-09-02
Kasman , Elina
MF 351 or AZ 351
Robert Black
2004-09-02
Did you word this correctly. I think Shiply makes Microposit MF and Hoechst
(also known as AZ) makes the AZ 351.
   Basically the only difference in developers is the surfact used, and
concentration of TMAOH. I would use the Shiply developer on the Shiply
resist. In my opinon, the best developer for Shiply 1813 is Shiply MF 319.



Hi all,

I would like to know what is the difference between Microposit MF 351
and Shipley AZ 351. The target photoresist is Shipley 1813.

Thank you all in advance.

Joolien



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing