BOE selective to etch glass, not Cr
2004-09-02
Parijat Bhatnagar
2004-09-06
David Nemeth
BOE selective to etch glass, not Cr
David Nemeth
2004-09-06
Don't neglect the possibility that the problem is pinholes in the Cr mask,
not the BOE.  Perhaps photoresist over the chrome mask could protect the
bulk of the mask, with the Cr defining the edges.

David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Parijat Bhatnagar
Sent: Thursday, September 02, 2004 12:04 PM
To: [email protected]
Subject: [mems-talk] BOE selective to etch glass, not Cr


Dear group,

I etched 7 microns of glass in 6:1 BOE which had 100 nm of Cr as a mask. I
could etch the glass but had some pitting in Cr. Does anybody has any
experience with etching in 60:1 BOE, or 30:1 BOE. Will that be a better
choice? Can I etch longer in more dilute BOE to still etch 7-8 microns of
glass but saving the Cr mask.

Sincerely,
Pari.

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
University Wafer
Process Variations in Microsystems Manufacturing