A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: problem in BCl3 etching
problem in BCl3 etching
2004-09-15
Maggie Q. Lai
problem in BCl3 etching
Maggie Q. Lai
2004-09-15
Hi, everybody, I had a problem in BCl3 etching on Si today.
When the purge after etching lasted for  40s ( which is supposed to be 2 min),
it stopped for some reason and we had no choice but to end the process.
But after we took out the sample, the surface looks yellowish, and become quite
conductive.
Did any body have similair problem before, do you know how to get rid of the
yellow stuff?The recipe we used is BCl3 50,, Cl2 50, O2 3.
THanks.

Maggie




_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

= = = = = = = = = = = = = = = = = = = =







reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
University Wafer
Mentor Graphics Corporation