Wet etching of silicon nitride?
2004-09-23
Sampo Tuukkanen
2004-09-23
Kirt Williams
2004-09-24
roy lam
2004-09-23
Kasman , Elina
Titanium oxide removal
2004-09-24
Balaji Lakshminarayanan
2004-09-24
Phillipe Tabada
2004-09-24
[email protected]
Wet etching of silicon nitride?
Sampo Tuukkanen
2004-09-23
Hi,

I would like to wet etch Si3N4 (LPCVD) to prevent the damages of silicon surface
during RIE.
BHF seems to be quite slow to that.


Best regards,

Sampo Tuukkanen, NanoScience Center, Jyväskylä.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics