MEMSnet Home: MEMS-Talk: selective etching of copper compared to Si
selective etching of copper compared to Si
2004-09-23
Laetitia Philippe
2004-09-23
Z. Jiang
2004-09-23
Brent Garber (2 parts)
selective etching of copper compared to Si
Z. Jiang
2004-09-23
hi,

   10% HNO3 will etch Copper very well.


   cheers

   jiang ziling

On Sep 23 2004, Laetitia Philippe wrote:

> Hi all
>
> do you know a good chemical etching of copper not damaging the silicone
> wafer underlying?
>
> Thanks a lot
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
University Wafer