MEMSnet Home: MEMS-Talk: sputter materials on Si02
sputter materials on Si02
2004-09-28
Federico
RIE Etching of Alumina
2004-09-28
Eric Zimney
2004-09-28
Brent Garber (2 parts)
2004-09-28
Kirt Williams
2004-09-29
Bruno Wacogne
sputter materials on Si02
Bruno Wacogne
2004-09-29
Hi Federico,

For example, you can use Ti or Cr which are usually used as adhesion layers
for coating silica with gold.

Good luck,

Bruno

At 10:35 28/09/2004 +0000, you wrote:
>Hi everybody
>
>There is anyone that could tell me which materials have the best adhesion
>properties for sputter on SiO2?
>
>thanks
>Federico
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
***********************************************
*                                             *
*   Bruno Wacogne                             *
*   Laboratoire d'Optique P.M. Duffieux       *
*   Faculté des Sciences et des Techniques    *
*   Route de Gray                             *
*   25030 Besançon cedex                      *
*                                             *
*   tel  (++33) 3 81 66 64 25                 *
*   fax  (++33) 3 81 66 64 23                 *
*   mel  [email protected]         *
*                                             *
* http://imfc.univ-fcomte.fr/lopmd/index.html *
* http://imfc.univ-fcomte.fr/                 *
*                                             *
***********************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
The Branford Group
University Wafer