Bulk Al2O3 properties
Imran Ghauri
2004-10-01
Dear Aamer Mahmood,

Please try the following link:

http://www.matweb.com/search/SpecificMaterial.asp?bassnum=BA1A

Muhammad Imran(PhD Student)
MEMS Lab University of Arkansas at Little Rock

--- Aamer Mahmood  wrote:

> Hello all,
> I need to know the mechanical, optical and thermal
> properties of bulk
> Al2O3. I am particularly interested in the yield
> strength of the material.
>
> One can easily find info for saphire but I am
> sputtering 1-3 um
> layers of Al2O3 at room temp.
>
> Any link/source to this kind of info will be
> appreciated.
>
> Thanks
>
> Aamer Mahmood
> Microsensors lab
> UT Arlington
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/
>




_______________________________
Do you Yahoo!?
Declare Yourself - Register online to vote today!
http://vote.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review
University Wafer