MEMSnet Home: MEMS-Talk: Photoresist for Patterning Aluminum
Photoresist for Patterning Aluminum
2004-10-05
Vivek Mukhatyar
2004-10-05
Shay Kaplan
teflon glue...
2004-10-05
Venkatachalam Chokkalingam
2004-10-05
William Lanford-Crick
2004-10-05
aasutosh dave
2004-10-05
rakesh babu
photopatternable silicone biocompatibility
2004-10-06
[email protected]
2004-10-05
Bill Moffat
Photoresist for Patterning Aluminum
Vivek Mukhatyar
2004-10-05
I was trying to spin coat aluminium with shipley 1818 negative resist.
 But when I used a wet etching solution the resist wasn't able to
withstand the etchant.  My patterns are on the scale of microns and
the best way to etch is through wet etching because i need to remove
alomost 300 micron thick aluminum.  Does anyone know the steps to spin
a thick layer of resist that will withstand the etchant that is made
up of Hcl and CuCl2.  I have SU-8 and 1818 to my disposal.  I also
need to remove the resist after the etching process.

Thank you,

Vivek Mukhatyar

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing