rakesh babu
eBeam evaporator problem
William Lanford-Crick
2004-10-07
You might also make sure the high voltage is at the level it should be.

Subject: [mems-talk] eBeam evaporator problem


Hi, all,   In my lab there is this 20 yr old NRC e-beam evaporator that
broke down lately. We had some urgent project needs be done and this busted
me.

The symptom is that the beam won't focus, and is very broad (~3/4"
diameter).  In effect, it heats up the edge of the crucible.  We can't melt
anything in the crucible, not even Au.
I have no clue how to fix this thing.  I'm guessing that the focusing
mechanism is busted.

anybody can throw some ideas? It's fairly urgent and thanks!


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
University Wafer