MEMSnet Home: MEMS-Talk: Plasma-Therm ICP
Plasma-Therm ICP
2004-10-07
Charlie Suh
2004-10-07
William Lanford-Crick
2004-10-08
Mark Fuller
2004-10-09
William Lanford-Crick
ANSYS Piezoresistive analysis
2004-10-10
rakesh babu
2004-10-11
Brent Garber (2 parts)
Feedthrough needed for a CVC evaporator
2004-10-07
Rajib Ahmed
2004-10-08
Joe Lonjin
Plasma-Therm ICP
William Lanford-Crick
2004-10-09
Hi Charlie,
We ship the pump out and have it rebuilt.  I'm unsure as to what precisely
they replace.
The pump eventually will shut itself off (or the ICP-RIE shuts it off) and
needs to be restarted.  Once this happens more frequently (i.e. either does
not restart or shuts off immediately after restart) we swap to another pump
and send the 1st out to be rebuilt.  It is several $1000s per rebuild.
-Bill

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Mark Fuller
Sent: Friday, October 08, 2004 9:46 AM
To: General MEMS discussion
Subject: RE: [mems-talk] Plasma-Therm ICP


At 12:41 PM 10/7/2004 -0500, you wrote:
>Hi Charlie,
>We have a single chamber Plasma Therm system, which is heavily used for
>III-Vs and SiC.  Most etching is with Cl2 or other chlorine-based gases and
>SF6.  We unfortunately have to have the turbo pump rebuilt every 6 months
or
>so (we are not sure why it fails so frequently).
>
What part of the pump gets replaced on the rebuild?
What indicates when you have to do a rebuild?


--
Mark Fuller
Microelectronics Fabrication Facility
Washington State University
Dana Hall 102
Pullman, WA  99164-2711
(509)335-1797
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
University Wafer
Tanner EDA by Mentor Graphics