> hello Mr Rocco
> I'm a student in metallurgy. could you please explain
> to me what application has Cr/TiN/Au on Si? I coated
> Cr/TiN on steel for corrosion resistance..
> thanks
> Afshar

Hi Afshar -

The only thing special about my request is the use of TiN as a diffusion
barrier to prevent the Au from mixing with the Si, especially at slightly
elevated temperatures.  This causes deterioration of both mechanical and
electrical properties.

-Tom

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
University Wafer
MEMStaff Inc.