I do not have stress-strain curves of SU-8, but I can measure
stress-strain curves of SU-8 coated on 4" (100mmm) Si wafer, please see
bellow similar measurements within my paper published at MRS Fall 2003,
section U11.29:

http://www.mrs.org/members/proceedings/fall2003/u/U11_29.pdf

Mircea


[email protected] wrote:
>
> We are doing thermal, mechanical simulation of SU-8 structure. I find the
> data sheet for SU-8 with modulus, CTE, Tg, etc. But I need the
> visco-elastic/plastic properties or the stress-strain curves at different
> temperatures (or atleast at room temp - 25C and molding temp - 175C) to
> complete the analysis. If you have these data or you know where I can find
> these data, please let me know, thanks!
> Gene
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

--

------------------------------
Mircea Capanu, Ph.D.
MicroSystemTechnology Engineer
R&D Gennum Corporation
P.O. Box 489, Station A,
Burlington, Ontario, Canada L7R 3Y3
or
Millenium Building, 970 Fraser Dr.,
Burlington, ON, Canada L7L 5P5
Phone: (905)-632-2999 ext. 2147
Fax:   (905)-632-2055
http://www.gennum.com
-------------------------------

*The information contained in this e-mail is confidential and
proprietary to
Gennum Corporation

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Addison Engineering
University Wafer